Looks good and should weather perfectly.

I use the same process on Galavnized parts as Rick (SS427) does... multiple Zinc rich paints including bright Galvanizing Zinc, cold Galvanizing zinc, and weldthrough ZINC and use a piece of ccrumpled up AL foil to give the crystalizing effect..
__________________
~JAG~
NCRS#65120
68 GTO HO 4 spd Alpine Blue /Parchment 2 owner car
#21783 71 Corvette LT1 45k miles Orig paint - Brandshatch Green - National Top Flight - last known 71 LT1 built.
71 Corvette LT1 42k miles Original paint - Black - black leather - only black LT1 known to exist.
NUMEROUS Lemans blue Camaros,
Monza Red and Daytona Yellow Corvettes
& a Chevelle or two...
Survivors, restored cars, & other photos
https://picasaweb.google.com/lh/myphotos
Reply With Quote
The Following 2 Users Say Thank You to firstgenaddict For This Useful Post:
RPOLS3 (03-03-2021), SS427 (03-03-2021)