View Single Post
  #138  
Old 07-28-2022, 01:30 AM
Oldss Oldss is offline
Yenko Premier Member
 
Join Date: Dec 2017
Location: Southwest WI
Posts: 134
Thanks: 1,341
Thanked 79 Times in 35 Posts
Default

Can I ask how you get DP90? I was a painter at a shop in the 1990’s. PPG at the time quite selling DP90, so we had to go to DP90LF. Of coarse, it had no adhesion to bare metal. You had to shoot a wash primer on first before the DPLF. I was surprised when you wrote that you were using DP. Thanks